Materials play an important role for the future needs toward higher strength or another dimension of speed. Daido Steel has extensive experience in manufacturing various kinds of material for many years. The DSALOY series, included more than 30%Ni, have higher strength at elevated temperature, high corrosion resistance, heat resistance and toughness. In addition, the DSALOY series have unique functional properties depending on the type and amount of alloy contained. We provide bars, wire rods, strips and forging products by our integrated system from melting to the finished products. We improve technological innovation constantly such as introducing a large vacuum induction melting furnace. Daido's "DSALOY" series will continue to challenge the creation of next generation innovation as high spec & high quality products.
★“DSALOY” is a registered trademark of Daido Steel Co., Ltd.

Font Size

Corrosion Resistant Alloys

 Corrosion Resistant Alloys Map

Chemical Composition

Classification Alloy UNS
(JIS)
Nominal Chemical Composition(wt%) Heat Treatment Tensile Strength(N/mm²) Elongation(%)
Ni Cr Mo Co Fe others
Corrosion Resistant Alloys DSALOY200 N02200
(NW2200)
≧99.0 - - - ≦0.4 C ≦ 0.15
Cu ≦ 0.2
A ≧380 ≧30
DSALOY201 N02201
(NW2201)
≧99.0 - - - ≦0.4 C ≦ 0.02
Cu ≦ 0.2
A ≧340 ≧30
DSALOY400 N04400
(NW4400)
≧63.0 - - - ≦2.5 Cu 28.0-34.0 A ≧480 ≧35
DSALOY
K-500
N05500
(NW5500)
bal. - - - ≦2.0 Cu 27.0-34.0
Al 2.2-3.2
Ti 0.35-0.85
ST+AG ≧830 ≧15
DSALOY 600 N06600
(NCF600)
≧72.0 14.0-
17.0
- - 6.0-
10.0
Cu ≦ 0.50 A ≧550 ≧30
DSA760 - bal. (38) - - - (Al 3.8) ST+AG ≧1,500 -
DSALOY
625
N06625
(NCF625)
≧58.0 20.0-
23.0
8.0-
10.0
≦1.0 ≦5.0 Al ≦ 0.40
Ti≦ 0.40
Nb+Ta 3.15-4.15
A ≧760 ≧30
DSALOY
C-276
N10276
(NW0276)
bal. 14.5-
16.5
15.0-
17.0
≦2.5 4.0-
7.0
W 3.0-4.5
V ≦0.35
A ≧690 ≧40
DSALOY
22
N06022
(NW6022)
bal. 20.0-
22.5
12.5-
14.5
≦2.5 2.0-
6.0
W 2.5-3.5
V ≦0.35
A ≧690 ≧45
DSALOY
CB3
N08020 32.0-
38.0
19.0-
21.0
2.0-
3.0
- bal. Cu3.0-4.0
Nb≦1.0
ST ≧550 ≧30
DSALOY
25-6MO
N08925 24.0-
26.0
19.0-
21.0
6.0-
7.0
- bal. Cu 0.5-1.5
N 0.15-0.25
ST ≧650 ≧35
DSP5 S35000 4.0-
5.0
16.0-
17.0
2.5-
3.2
- bal. Mn 0.5-1.25 ST+AG ≧1,300 ≧4

A:Annealing ST:Solution heat Treatment AG:Aging

Features Applications

Classification Alloy Features Applications
Corrosion Resistant Alloys DSALOY
200
Good mechanical properties, Excellent corrosion resistance to many corrosive media Production facilities for foods, caustic soda, chemicals and synthetic fibers, Electrical and electronic components
DSALOY
201
Excellent cold workability, No embrittlement by carbon above 300℃ Similar applications to DSALOY200, Cold deep-drawn parts
DSALOY
400
High strength, Good workability, Excellent corrosion resistance to many corrosive environments Facilities of seawater desalination, salt production and oil refining, Marine construction coverings, Heat exchangers
DSALOY
K-500
Similar corrosion resistance to DSALOY400, Higher strength than DSALOY400, Completely non- magnetic even at -100℃ Parts requiring higher strength than DSALOY400, Oil-drilling tools, Corrosion resistant valves and springs, Rotary pumpshafts, Fasteners
DSALOY
600
Good oxidation resistance at high temp. , Corrosion resistance to pure water/alkali/Cl - ion (SCC*) Equipment for chemical and food production, Heat exchangers, Electronic components
DSA760
High hardness equivalent to that of martensite stainless steel, High corrosion resistance, Non magnetic Medical scissors, Dental drills, Automotive turbo parts
DSALOY
625
High strength without heat treatment, Excellent corrosion resistance in a wide range of severe corrosive environments Chemical product manufacturing facilities, Aerospace parts, Seawater treatment facilities
DSALOY
C-276
Excellent corrosion resistance in a wide range of severe corrosive environments, Good weldability Flue-gas desulfurization equipment (FGD), Chemical industrial equipment, Pulp and paper mill facilities
DSALOY
22
Excellent acid corrosion resistance to many types of corrosion such as SCC, pitting and intergranular corrosion Chemical manufacturing equipment, Combustion gas FGD, Bleaching equipment at paper mills
DSALOY
CB3
Excellent acid corrosion resistance to many types of corrosion such as pitting, crevice corrosion and intergranular corrosion Chemical and petrochemical product manufacturing equipment parts (tanks, heat exchangers, piping, pumps, valves)
DSALOY
25-6MO
Corrosion resistance to pitting, crevice corrosion and non-oxidizing acids such as sulfuric acid and phosphoric acid Tubes for petrochemical industry and seawater cooling equipment, Salt production plant parts, Biochemical equipment parts
DSP5 Similar strength to martensitic stainless steel , Excellent corrosion resistance to non-oxidizing acid Bellows , Automotive parts , Various sealing parts

*SCC(Stress Corrosion Cracking)

Specifications・Available Products

Classification Alloy Available Products Specifications
Bar Wire rod Strip ASTM JIS
Corrosion Resistant Alloys DSALOY
200
B160
B162
G4902
H4553
H4554
DSALOY
201
B160
B162
G4902
H4553
H4554
DSALOY
400
B127
B164
B564
G4902
H4553
H4554
DSALOY
K-500
- - B865 H4553
DSALOY
600
B166
B168
B564
G4901
G4902
DSA760 - - -
DSALOY
625
B443
B446
B564
G4901
G4902
DSALOY
C-276
B564
B574
B575
G4902
H4553
H4554
DSALOY
22
B564
B574
B575
G4902
H4553
H4554
DSALOY
CB3
- B472
B473
-
DSALOY
25-6MO
- B472
B649
-
DSP5 - - A693 -

◎:Standard ◯:Available ー:Not available